Step 1:
Ensure the area to be repaired is clean, dry, and free of grease. Remove any loose or protruding particles if necessary.
Ensure the area to be repaired is clean, dry, and free of grease. Remove any loose or protruding particles if necessary.
Step 3:
Apply the Special Scraper, “small” with the round sides and remove scratches in even strokes from top to bottom.
Apply the Special Scraper, “small” with the round sides and remove scratches in even strokes from top to bottom.
Step 4:
Use the Cork Sanding Block with Felt Pad and Sandpaper, “wet” (500-1000 grit) for pre-sanding. Use sufficient water and always sand in the longitudinal direction of the profile, no circular movements.
Use the Cork Sanding Block with Felt Pad and Sandpaper, “wet” (500-1000 grit) for pre-sanding. Use sufficient water and always sand in the longitudinal direction of the profile, no circular movements.
Step 5:
Use the Cork Sanding Block with Felt Pad and Micro Sanding Paper (1.800-4.000 grit) for polishing. Use sufficient water and always sand in the longitudinal direction of the profile, no circular movements.
Use the Cork Sanding Block with Felt Pad and Micro Sanding Paper (1.800-4.000 grit) for polishing. Use sufficient water and always sand in the longitudinal direction of the profile, no circular movements.
Step 6:
Adjust gloss level using the Felt Pad and Polishing Paste, “fine”.
Adjust gloss level using the Felt Pad and Polishing Paste, “fine”.
Step 7:
Clean with the Special Cloth or Cotton Cloth.
Clean with the Special Cloth or Cotton Cloth.